Formation mechanism of strontium cobaltite containing equimolar amounts of Sr and Co from SrCO3 and Co3O4
Abstract
Strontium cobaltite containing equimolar amounts of Sr and Co was produced by heating the mixture of SrCO3 and Co3O4 starting materials with a mole ratio of 1:0.333 under dynamic air atmosphere. The chemical reactions occurred during heating were determined and the intermediate and final products obtained at each critical temperature were characterized using TG/DTA-MS, ICP-OES, XRD and FT-IR analytical techniques. The volumetric analysis method (iodometric titration) and carbonation process were carried out to determine the oxygen stoichiometry of strontium cobaltite.
Collections