Basit öğe kaydını göster

dc.contributor.authorŞahin, Meryem
dc.contributor.authorMUTLU, İlven
dc.contributor.authorÜNALAN, Fatma
dc.date.accessioned2023-02-21T09:58:49Z
dc.date.available2023-02-21T09:58:49Z
dc.date.issued2022
dc.identifier.citationŞahin M., ÜNALAN F., MUTLU İ., "Corrosion, ion release, and surface hardness of Ti-6Al-4V and cobalt-chromium alloys produced by CAD-CAM milling and laser sintering", Journal of Prosthetic Dentistry, cilt.128, sa.3, 2022
dc.identifier.issn0022-3913
dc.identifier.othervv_1032021
dc.identifier.otherav_394c0f8c-840d-4bc1-9144-a3011334c6ea
dc.identifier.urihttp://hdl.handle.net/20.500.12627/187972
dc.identifier.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85135515759&origin=inward
dc.identifier.urihttps://doi.org/10.1016/j.prosdent.2022.06.011
dc.description.abstract© 2022 Editorial Council for the Journal of Prosthetic DentistryStatement of problem: How the corrosion properties of cobalt-chromium (Co-Cr) and Ti (Ti-6Al-4V) alloys, frequently used in dental prostheses, are affected by different production methods is unclear. Purpose: The purpose of this in vitro study was to compare Co-Cr and Ti-6Al-4V alloys produced by computer-aided design and computer-aided manufacturing (CAD-CAM) milling or laser sintering in terms of corrosion, ion release, and surface hardness. Material and methods: Co-Cr and Ti-6Al-4V specimens were produced by CAD-CAM milling and direct metal laser sintering/selective laser sintering techniques. Testing included Vickers hardness and then open circuit potential (OCP), Tafel extrapolation, and static immersion to determine the corrosion behavior. The study used an inductively coupled plasma mass spectrometer to measure ion release. The data were analyzed by using the Kruskal-Wallis and Mann-Whitney U tests, with Bonferroni correction (α=.05). Results: The Ti-6Al-4V laser-sintered group showed the highest Vickers hardness value (P.05). Conclusions: Ti-6Al-4V alloys may be a good alternative for patients with Co-Cr allergies, but as per the results of this study, Co-Cr still seems more suitable for clinical use.
dc.language.isoeng
dc.subjectDİŞ HEKİMLİĞİ, ORAL CERRAHİ VE TIP
dc.subjectKlinik Tıp (MED)
dc.subjectDiş Hekimliği
dc.subjectTıp
dc.subjectKlinik Tıp
dc.subjectAğız Cerrahisi
dc.subjectSağlık Bilimleri
dc.titleCorrosion, ion release, and surface hardness of Ti-6Al-4V and cobalt-chromium alloys produced by CAD-CAM milling and laser sintering
dc.typeMakale
dc.relation.journalJournal of Prosthetic Dentistry
dc.contributor.departmentİstanbul Üniversitesi , ,
dc.identifier.volume128
dc.identifier.issue3
dc.contributor.firstauthorID4110450


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster