Basit öğe kaydını göster

dc.contributor.authorHAZIR, Ender
dc.contributor.authorKOÇ, Küçük Hüseyin
dc.date.accessioned2021-03-03T17:46:44Z
dc.date.available2021-03-03T17:46:44Z
dc.date.issued2019
dc.identifier.citationHAZIR E., KOÇ K. H. , "EVALUATION OF WOOD SURFACE COATING PERFORMANCE USING WATER BASED, SOLVENT BASED AND POWDER COATING", MADERAS-CIENCIA Y TECNOLOGIA, cilt.21, sa.4, ss.467-480, 2019
dc.identifier.issn0718-221X
dc.identifier.othervv_1032021
dc.identifier.otherav_4b636716-3b50-4383-b44f-4989b78fbd80
dc.identifier.urihttp://hdl.handle.net/20.500.12627/54106
dc.identifier.urihttps://doi.org/10.4067/s0718-221x2019005000404
dc.description.abstractThe objective of this study was to evaluate the surface coating performance using water base, solvent base and powder coating on medium density fiberboard. Samples were coated using water-base, solvent-base and powder coating. Coating performance was performed by using adhesion strength, surface coating hardness, layer thickness and rapid deformation test. The results were analyzed with two different statistical methods. Adhesion strength, layer thickness and surface hardness were determined by using ANOVA analysis, while results of rapid deformation test were analyzed by using Kruskal-Wallis method. According to these results, coating type was effective factor on the adhesion strength, surface coating hardness, layer thickness and rapid deformation test. Water-based painting application for adhesion strength and impact deformation resistance were higher than solvent-based coating. In the powder coating application, although surface coating hardness was higher than solvent and water base coating application, rapid deformation results were lower than solvent and water base coating applications. Adequacy of models was performed R-square (R-2) and Adjusted R-square (Adj-R-2) values. R-2 values of adhesion strength, layer hardness and film layer thickness were 93,60 %; 95,33 % and 73,90 %, respectively. Adj-R-2 values of adhesion strength, layer hardness and film layer thickness were 93,45 %; 95,23 % and 73,30 %, respectively.
dc.language.isoeng
dc.subjectMALZEME BİLİMİ, KAĞIT & AHŞAP
dc.subjectMalzeme Bilimi
dc.subjectMühendislik, Bilişim ve Teknoloji (ENG)
dc.subjectMühendislik ve Teknoloji
dc.titleEVALUATION OF WOOD SURFACE COATING PERFORMANCE USING WATER BASED, SOLVENT BASED AND POWDER COATING
dc.typeMakale
dc.relation.journalMADERAS-CIENCIA Y TECNOLOGIA
dc.contributor.departmentİstanbul Üniversitesi-Cerrahpaşa , Orman Fakültesi , Orman Endüstrisi Makinaları Ve İşletme Ana Bilim Dalı
dc.identifier.volume21
dc.identifier.issue4
dc.identifier.startpage467
dc.identifier.endpage480
dc.contributor.firstauthorID271147


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster