dc.contributor.author | Sancakli, Erkan | |
dc.contributor.author | Ozel, Sevda | |
dc.contributor.author | Yıldız, Esra | |
dc.contributor.author | Sancakli, Hande | |
dc.contributor.author | Erdemir, Uğur | |
dc.contributor.author | Yucel, Taner | |
dc.contributor.author | Eren, Meltem Mert | |
dc.date.accessioned | 2021-03-04T19:49:20Z | |
dc.date.available | 2021-03-04T19:49:20Z | |
dc.date.issued | 2014 | |
dc.identifier.citation | Erdemir U., Sancakli H., Sancakli E., Eren M. M. , Ozel S., Yucel T., Yıldız E., "Shear bond strength of a new self-adhering flowable composite resin for lithium disilicate-reinforced CAD/CAM ceramic material.", The journal of advanced prosthodontics, cilt.6, ss.434-43, 2014 | |
dc.identifier.issn | 2005-7806 | |
dc.identifier.other | av_91a3a264-9d9d-4e8d-9492-a7a3ca4c4c7d | |
dc.identifier.other | vv_1032021 | |
dc.identifier.uri | http://hdl.handle.net/20.500.12627/98243 | |
dc.identifier.uri | https://doi.org/10.4047/jap.2014.6.6.434 | |
dc.description.abstract | PURPOSE. The purpose of this study was to evaluate and compare the effects of different surface pretreatment techniques on the surface roughness and shear bond strength of a new self-adhering flowable composite resin for use with lithium disilicate-reinforced CAD/CAM ceramic material. MATERIALS AND METHODS. A total of-one hundred thirty lithium disilicate CAD/CAM ceramic plates with dimensions of 6 mm x 4 mm and 3 mm thick were prepared. Specimens were then assigned into five groups (n=26) as follows: untreated control, coating with 30 mu m silica oxide particles (Cojet (TM) Sand), 9.6% hydrofluoric acid etching, Er:YAG laser irradiation, and grinding with a high-speed fine diamond bur. A self-adhering flowable composite resin (Vertise Flow) was applied onto the pre-treated ceramic plates using the Ultradent shear bond Teflon mold system. Surface roughness was measured by atomic force microscopy. Shear bond strength test were performed using a universal testing machine at a crosshead speed of 1 mm/min. Surface roughness data were analyzed by one-way ANOVA and the Tukey HSD tests. Shear bond strength test values were analyzed by Kruskal-Wallis and Mann-Whitney U tests at alpha=.05. RESULTS. Hydrofluoric acid etching and grinding with high-speed fine diamond bur produced significantly higher surface roughness than the other pretreatment groups (P<.05). Hydrofluoric acid etching and silica coating yielded the highest shear bond strength values (P<.001). CONCLUSION. Self-adhering flowable composite resin used as repair composite resin exhibited very low bond strength irrespective of the surface pretreatments used. | |
dc.language.iso | eng | |
dc.subject | Klinik Tıp (MED) | |
dc.subject | Sağlık Bilimleri | |
dc.subject | DİŞ HEKİMLİĞİ, ORAL CERRAHİ VE TIP | |
dc.subject | Klinik Tıp | |
dc.subject | Tıp | |
dc.subject | Diş Hekimliği | |
dc.title | Shear bond strength of a new self-adhering flowable composite resin for lithium disilicate-reinforced CAD/CAM ceramic material. | |
dc.type | Makale | |
dc.relation.journal | The journal of advanced prosthodontics | |
dc.contributor.department | İstanbul Üniversitesi , , | |
dc.identifier.volume | 6 | |
dc.identifier.issue | 6 | |
dc.identifier.startpage | 434 | |
dc.identifier.endpage | 43 | |
dc.contributor.firstauthorID | 72302 | |